Skip to main content

Material selection6 min read

SUS 317L pipe for Japan: S31703 or S31700?

A Japanese drawing may say SUS 317L while the supplier offer says UNS S31700. Check carbon, molybdenum, PREN and the mill certificate before accepting the pipe.

Junda stainless steel pipe product photo

Junda Pipe

Published Reviewed

SUS 317L is the low-carbon 317 grade. Its UNS number is S31703, not S31700. UNS S31700 is standard 317, which allows up to 0.08% carbon. When a Japanese drawing says SUS 317L and an offer says S31700, treat the two as different grades until the carbon limit and the product standard are verified on the mill certificate.

This guide is for the buyer or piping engineer comparing a Japanese drawing with an overseas mill offer. It answers one question: which designation belongs on the order, and what document proves the delivered pipe matches it.

What is the difference between SUS 317L and UNS S31700?

SUS 317L is the JIS designation for low-carbon 317L, and it maps to UNS S31703. UNS S31700 is standard 317 with a higher carbon ceiling. Both contain 3.0% to 4.0% molybdenum, so a chemistry report alone can look similar. The carbon limit and the governing product standard separate them.

DesignationCarbon, maxMolybdenumUNS numberHow to write it on the order
SUS 317L / 317L0.03%3.0% to 4.0%S31703317L (UNS S31703)
3170.08%3.0% to 4.0%S31700317 (UNS S31700)
316L, for comparison0.03%2.0% to 3.0%S31603316L (UNS S31603)

Table: Designations that are often treated as interchangeable. The carbon ceiling and the product standard must match the drawing; the molybdenum range alone does not identify the grade. Values follow the ASTM A312/A312M and A213/A213M grade tables and the JIS designation for 317L. Confirm the edition named on the project specification.

The practical error is a quotation that says "317L" in the description and "S31700" in the certificate or the drawing reference. That offer can be standard 317. Ask the supplier to state the grade and the UNS number in the same line, then compare both with the purchase order.

Why does the carbon difference matter in chloride service?

Molybdenum raises resistance to pitting, and carbon changes what happens near a weld. 317L holds carbon at 0.03% or below to limit chromium carbide precipitation in the heat-affected zone. Standard 317 can serve unwelded or less severe duty, but it is not a drop-in replacement for a 317L drawing.

PREN = Cr + 3.3 Mo + 16 N, with the elements entered in weight percent. At 18.5% Cr, 3.5% Mo and 0.05% N, PREN is 30.9. At 2.5% Mo with the same Cr and N, it is 27.6. The 3.3-point step comes from molybdenum alone. Calculate the number from the heat analysis and state the basis; a PREN value without chemistry is not a corrosion test.

The number is a screening tool, not a service guarantee. Chloride concentration, temperature, dissolved oxygen, flow velocity, stagnation, crevice geometry and cleaning practice can all move the failure threshold. A 317L pipe that suits a moderate chloride stream can still pit in a stagnant, chlorinated or high-temperature section. For seawater or hot concentrated chloride, compare 317L with super duplex or 6% Mo grades instead of assuming that more molybdenum solves every case.

Low carbon also does not replace the welding procedure. The fabricator still controls heat input, interpass temperature, filler metal and post-weld cleaning. A 317L certificate with 0.02% carbon does not prove that a field weld will pass a corrosion test.

What should a 317L purchase order say?

Write the grade, UNS number, product standard and edition, size, wall basis, heat treatment, test scope and certificate type on the order. An offer that says only 317L leaves the carbon limit, the inspection standard and the document package open.

Order fieldWrite thisWhy it matters
Grade and UNS317L (UNS S31703)Prevents an S31700 substitution
Product standardASTM A312/A312M-25 for pipe, A213/A213M-25 for tube, or the JIS standard named on the drawingSets dimensions, tests and tolerances
Size and wallNPS and schedule, or OD and average or minimum wallFixes the bore and the pressure basis
ChemistryC 0.03% max, Cr 18% to 20%, Ni 11% to 15%, Mo 3.0% to 4.0%, N reportedMakes the grade auditable
Heat treatmentSolution anneal and cooling methodRestores corrosion resistance after forming
InspectionHydrostatic or non-destructive test, mechanical tests and PMIDefines the evidence the mill must supply
CertificateEN 10204 Type 3.1, or Type 3.2 where the project requires itTies the heat number to the delivered pipe

Table: Minimum purchase-order fields for a 317L line item. Add any project-specific impact, corrosion or third-party inspection requirements rather than relying on the grade name.

If the drawing uses JIS notation, keep the JIS grade and add the ASTM or UNS cross-reference as a second line. Do not replace the governing standard with a cross-reference. The product standard decides the dimensions and the test methods; the UNS number only identifies the alloy.

How do you verify a supplier's 317L offer?

Compare the mill certificate to the order line, not to the supplier's catalogue. The certificate must identify the heat, the grade, the product standard and the actual analysis. A PMI check on delivery confirms the alloy family but does not measure carbon.

  1. The certificate names 317L or UNS S31703, not S31700.
  2. Carbon is reported at 0.03% or below.
  3. Molybdenum is within 3.0% to 4.0%.
  4. Chromium and nickel are within the 317L range.
  5. The product standard and edition match the drawing.
  6. The heat-treatment record states the solution anneal and cooling method.
  7. Mechanical tests and the specified non-destructive test are reported for the same heat or lot.
  8. The heat number on the certificate matches the marking on the pipe.

If any line is missing, ask for a revised certificate before the pipe is released. A certificate that reports only the ladle analysis without the product analysis may not represent the delivered wall. The material certificate traceability guide explains how EN 10204 Type 3.1 and Type 3.2 documents differ.

What changes when the supplier is outside Japan?

A Japanese drawing may name SUS 317L and a JIS product standard, while an overseas mill may quote ASTM A312 TP317L. The alloy can match, but the standard, tolerances, inspection and certificate do not become equivalent by translation. State which standard governs and which alternative you will accept.

Ask the supplier for a written deviation list against the drawing, the governing standard on the offer, the certificate type and the third-party inspection option. If the project requires a JIS mark or a Japanese witness, confirm that the mill and the inspection body can provide it before the order is placed. Do not accept a certificate that lists only the UNS number when the drawing names a JIS grade and standard.

Junda quotes 317L pipe to the standard, size and inspection scope stated on the enquiry. The 317L seamless pipe page gives the product route, and the PREN calculation guide shows how to screen the heat analysis. Send the drawing line, the grade and the required certificate to the contact page for a technical quotation.

FAQ: SUS 317L and UNS S31700

Is SUS 317L the same as UNS S31700?

No. SUS 317L is the low-carbon grade and maps to UNS S31703. UNS S31700 is standard 317 with a higher carbon ceiling. Check the carbon limit and the product standard before accepting an S31700 offer against a SUS 317L drawing.

What is the UNS number for 317L?

UNS S31703. The common error is to write S31700, which is 317, not 317L. The purchase order and the mill certificate should both say 317L or S31703.

Does 317L resist seawater?

Not in every condition. 317L has more molybdenum than 316L, but pitting resistance still depends on chloride concentration, temperature, oxygen, flow and crevices. Calculate PREN from the heat analysis and verify the actual service condition; super duplex or 6% Mo grades may be required.

Questions buyers ask

Is SUS 317L the same as UNS S31700?

No. SUS 317L is the low-carbon grade and maps to UNS S31703. UNS S31700 is standard 317 with a higher carbon ceiling. Check the carbon limit and the product standard before accepting an S31700 offer against a SUS 317L drawing.

What is the UNS number for 317L?

UNS S31703. The common error is to write S31700, which is 317, not 317L. The purchase order and the mill certificate should both say 317L or S31703.

Does 317L resist seawater?

Not in every condition. 317L has more molybdenum than 316L, but pitting resistance still depends on chloride concentration, temperature, oxygen, flow and crevices. Calculate PREN from the heat analysis and verify the actual service condition; super duplex or 6% Mo grades may be required.


Links to standards bodies and material producers are provided for reference. Confirm the applicable edition, project requirements and acceptance documents for each order.

Share this article

Continue with AI

Read as Markdown

Bring this article into your own conversation.

Preferred Sources

Keep up with Junda Pipe on Google.

Availability depends on your account and region.

Material selection

Selecting austenitic stainless steel pipe

Select austenitic stainless steel pipe by fluid, temperature, product standard and inspection scope using the screening table for 316L, 321, 347H and 904L.

Material selection

316L seamless pipe in welded service

Order 316L seamless pipe when welded lines cannot be post-weld annealed: how 0.030% max carbon limits sensitization and what the weld procedure still controls.

Material selection

904L pipe for acid service

Evaluate UNS N08904 (904L) pipe for sulfuric and phosphoric acid lines: record the five operating variables, read iso-corrosion curves and check ASTM A312.

Ready to discuss your pipe requirements?

Send the grade, dimensions, quantity and required documents with your enquiry.