316L welded service: one band, one number

The L in 316L covers the band beside the weld — carbon 0.030 % maximum, chromium stays in the metal. It does not cover the bore surface, the procedure or…

Format
Short
Published
Duration
50 sec
Language
English
Full explainer series: Junda Explainers

About this video

This explainer is educational. It explains the published limits and the order fields for the topic; confirm the grade, standard, size, condition, inspection and documents with Junda for each order.

Chapters

Each chapter opens the video at that point on YouTube.

  1. 0:00

    A 316L pipe leaves the mill with no weld anywhere in its body.

    In welded service, every joint in that line is made later, somewhere else. The letter L answers one question about that joint. Your line asks three.

  2. 0:14

    On site, two ends are bevelled, lined up and joined with a girth weld.

    The arc heats a band on both sides of the bead, and that band cools in a hurry. Inside that band, carbon and chromium can combine at the grain boundaries, and the metal beside them loses chromium.

  3. 0:30

    A heat with more carbon loses that chromium, and nothing in service puts it back.

    The joint has a second side, and this is the side the L cannot cover. Weld the root without a purge and an oxide forms on the bore as the metal cools. The full explainer follows the joint from the mill gate to the cleaning cycle.

Specify the pipe or tube for your project

Send the grade, standard, OD × wall × length, wall basis, quantity, inspection and documents with your enquiry.