317L vs 316L: one point of molybdenum is 3.3 PREN

317L vs 316L: same mill, same size, same standards. One carries more molybdenum, and one point of molybdenum is 3.3 PREN.

Format
Short
Published
Duration
51 sec
Language
English
Full explainer series: Junda Explainers

About this video

This explainer is educational. It separates the L (a carbon limit that answers welding) from the molybdenum (the chloride screening step), uses the published screening order and IMOA's PREN formula, and leaves the measured chemistry to the EN 10204 type 3.1 certificate. PREN is a screening number, not a corrosion test; confirm grade, standard, size, tests and documents on the quotation for each order.

Chapters

Each chapter opens the video at that point on YouTube.

  1. 0:00

    317L vs 316L: one step of molybdenum

    317L vs 316L: same mill, same size, same test record. One carries more molybdenum in the steel. What does that buy?

  2. 0:10

    Cold drawing pulls the tube through a die

    Cold drawing pulls the tube through a die, over a fixed mandrel. The wall thins and the bore is set. Both grades run it.

  3. 0:18

    316L is the baseline: 2 to 3 % molybdenum

    316L is the baseline: low carbon, and 2 to 3 percent molybdenum. The low carbon answers welding. It does not answer pitting in chloride. So ask what the extra molybdenum answers, not which grade is better.

  4. 0:32

    The step is measured, not chemical immunity

    In chloride service, the attack starts at the wall. Chloride, oxygen, pH, velocity, stagnation and cleaning: the published service list. Add design temperature, and the piping code that governs the line. None of that is in the grade name.

  5. 0:46

    The full explainer follows that step

    The full explainer follows that step into the order line.

Specify the pipe or tube for your project