347 vs 347H stainless steel pipe: what the H changes

347 vs 347H stainless steel pipe: 347 allows up to 0.08 % carbon, 347H is held between 0.04 and 0.10 %, and that window is what changes the anneal, the grain…

Format
Explainer
Published
Duration
2 min 41 sec
Language
English
Full explainer series: Junda Explainers

About this video

This explainer is educational. It explains the published limits and the order fields for the topic; confirm the grade, standard, size, condition, inspection and documents with Junda for each order.

Chapters

Each chapter opens the video at that point on YouTube.

  1. 0:00

    347 vs 347H stainless steel pipe: what the H changes

    347 vs 347H stainless steel pipe: one letter on the order, two different steels. Both are niobium-stabilized. The H changes what the mill must prove.

  2. 0:13

    What the H changes on a 347H stainless steel pipe order

    Three things change with the H. The carbon window, the annealing temperature and the grain size. None of them is the outside diameter, and all three have to be proved.

  3. 0:24

    Carbon and niobium: the 0.04 to 0.10 % window and ten times the carbon

    347 allows carbon up to 0.08 percent, with no minimum. 347H is held between 0.04 and 0.10 percent, and that floor is the point. Below 0.04, the published creep-rupture strength drops away. Niobium is the element that holds that carbon in place. The published rule is ten times the carbon, or more. At the top of each window, that is 0.8 percent niobium, and 1.0 percent. So the H is not a suffix. It moves the alloy floor.

  4. 1:00

    Niobium carbide on the grain boundary and the 427 to 816 °C sensitization range

    Inside the wall, the metal is a field of grains and boundaries. Niobium ties the carbon up inside the grain, as niobium carbide. That is the whole job: keep chromium carbide off the boundaries. Every boundary is a path that a corrosive service can follow. Now the part a data sheet hides. If the niobium is short, or the anneal is cut, chromium carbide forms on the boundary. Between 427 and 816 degrees, that boundary is where sensitization starts.

  5. 1:32

    Solution annealing and ASTM grain size on the 347H mill certificate

    347H is solution annealed higher, typically 1050 to 1100 degrees. And the grain size is specified at ASTM 7, or coarser. Coarse grains and high carbon are what carry the load at temperature. So the mill certificate has to carry three things, not one. The carbon value, the annealing chart, the grain size. Overlapping chemistry alone is not dual certification.

  6. 2:00

    ASTM A312 pipe or A213 tube: writing the 347H enquiry

    The same grade is ordered as A312 pipe for the line, or A213 tube for the exchanger. Where creep governs, the H grade is the one written into the tube specification. None of this changes the outside diameter or the wall. Those come from the order and the design code, not from the letter. So the enquiry names the grade and its designation. The standard and the product form, and the condition. Then the documents and the tests, named one by one. Everything the quotation has to confirm in writing. Send the grade, the standard and the size, and we confirm the pipe against your specification.

Specify the pipe or tube for your project