Skip to main content

Short · 55 s

C-276 corrosion data: 0.1 mm a year is not zero #shorts

A C-276 corrosion rate is measured on a specimen in one bath at one concentration and one temperature: 0.1 mm a year is the line, and twenty years on it is t…

Format
Short
Published
Duration
55 sec
Language
English
Full explainer series: Junda Explainers

About this video

This explainer is educational. It explains the published limits and the order fields for the topic; confirm the grade, standard, size, condition, inspection and documents with Junda for each order.

Chapters

Each chapter opens the video at that point on YouTube.

  1. 0:00

    Hastelloy C-276 pipe corrosion data starts at one tenth of a millimetre a year.

    That line is measured in a bath like this one, not on your line. Junda's published pages list C-276 for sulfuric acid condensers and acetic acid reactors.

  2. 0:18

    There the wall is a tube: process inside, cooling water outside.

    The data is about that wall, and only that wall. A corrosion rate comes from a specimen in a bath. Here: hydrochloric acid at twenty percent, boiling, and the line at one tenth of a millimetre a year.

  3. 0:34

    Add ferric ions, air or solids, and this is no longer the test.

    One tenth of a millimetre a year is two millimetres in twenty years. The chart measures the rate. Your design life sets the years. So the wall is where a reading becomes a decision. The full explainer reads the specimen, the wall and the order. It is on our channel.

Specify the pipe or tube for your project