Solution annealing and delivery condition
Hastelloy C-276 is supplied solution annealed and rapidly quenched. The anneal is typically in the 1,120–1,150 °C range; the exact temperature, hold and cooling are recorded on the heat-treatment chart and confirmed against the ordered standard.
C-276 depends on a balanced nickel-molybdenum-chromium matrix with tungsten. Slow cooling or a missed anneal can precipitate intermetallic phases and reduce corrosion resistance, so the heat-treatment record is part of the material release.
- Solution-annealed and water-quenched condition
- Pickled and passivated finish where specified
- PMI to confirm Cr, Mo, W and Fe
- Hydrostatic, UT/ET and mechanical tests agreed per order